logo
Home > Products > Aluminum Metal Powder >
High Strength Weight Ratio AlSi10Mg Aluminum Alloy Powder For Additive Manufacturing

High Strength Weight Ratio AlSi10Mg Aluminum Alloy Powder For Additive Manufacturing

Place of Origin:

China

Brand Name:

Zoli

Certification:

ISO CE

Model Number:

AlSi10Mg

Contact Us
Request A Quote
Product Details
Boiling Point:
2467 °C
Solubility In Water:
Insoluble
Electrical Conductivity:
38.2 MS/m
Bulk Density:
2.5-3.5 G/cm3
Thermal Conductivity:
237 W/mK
Molecular Weight:
26.98 G/mol
Storage Conditions:
Store In A Cool, Dry Place
Material:
Aluminum
Safety Information:
Harmful If Swallowed, Causes Skin And Eye Irritation
Country Of Origin:
China
Elongation:
Depends On The Specific Metal Alloy Used
Sintering Atmosphere:
Nitrogen Or Hydrogen
Feature:
Sliver White Powder
Dangerous:
Flammable
Payment & Shipping Terms
Minimum Order Quantity
1kg
Packaging Details
vacuum,plastic and iron barrel
Delivery Time
within 30days
Payment Terms
L/C,T/T,Western Union
Supply Ability
500ton per year
Product Description
1. Overview and Introduction

AlSi10Mg is a near-eutectic aluminum-silicon-magnesium alloy that is arguably the most widely used and well-understood aluminum powder in the field of metal additive manufacturing (AM), particularly in Laser Powder Bed Fusion (LPBF) processes. Its popularity stems from an excellent combination of good printability, high strength-to-weight ratio, thermal properties, and cost-effectiveness.

Originally developed for traditional casting (where it is known as A360), its composition is exceptionally well-suited for the rapid solidification characteristics of 3D printing, resulting in fine, stable microstructures and superior mechanical properties compared to its cast counterpart.

2. Chemical Composition (Typical Weight %)

The composition is precisely controlled to ensure optimal performance. A standard composition conforming to standards like ASTM B928 / AMS 4345 is:

Element Content (%) Role and Effect
Aluminum (Al) Balance Base metal, provides the matrix.
Silicon (Si) 9.0 - 11.0% Primary alloying element. Lowers melting point, improves fluidity, reduces hot cracking, and enhances hardness and strength through dispersion strengthening.
Magnesium (Mg) 0.2 - 0.45% Enables precipitation hardening (age hardening). Forms Mg₂Si precipitates during heat treatment, significantly increasing strength.
Iron (Fe) ≤ 0.15% Impurity. Kept low to prevent the formation of brittle intermetallic phases that can reduce toughness.
Manganese (Mn) ≤ 0.45% Sometimes added to modify iron-containing phases, making them less detrimental.
Other Impurities ≤ 0.05% each Elements like Copper (Cu), Zinc (Zn), Titanium (Ti), etc., are strictly controlled to ensure consistent material behavior and final properties.
3. Key Characteristics and Properties
  • Excellent Printability: The Al-Si eutectic system has a relatively wide freezing range, which minimizes residual stresses and the tendency for hot cracking (solidification cracking) during the LPBF process. This makes it one of the most forgiving and reliable aluminum alloys to print.
  • Good Strength and Hardness: In the "as-printed" condition, it offers decent mechanical properties. However, its true potential is unlocked through heat treatment (see Section 5).
  • High Thermal Conductivity: Exhibits good thermal conductivity, making it suitable for applications like heat exchangers, cooling plates, and electronic enclosures.
  • Low Density (~2.67 g/cm³): Provides a high strength-to-weight ratio, which is critical for aerospace, automotive, and robotics applications where weight savings are paramount.
  • Good Corrosion Resistance: Offers respectable resistance to atmospheric corrosion, similar to other aluminum-silicon alloys.
4. Powder Characteristics (Crucial for AM)

The quality of the powder is as important as its chemical composition. Key powder properties include:

  • Particle Size Distribution (PSD): Typically ranges from 15 to 63 microns for standard LPBF systems. Some systems may use a tighter distribution (e.g., 20-45 µm) for finer detail resolution.
  • Morphology: Particles must be spherical to ensure good flowability, which is essential for creating a uniform, dense powder bed layer after layer. Non-spherical particles can cause poor recoating, leading to defects.
  • Flowability: Measured by Hall Flowmeter (e.g., < 35 s/50g). Good flowability ensures a consistent and reliable printing process.
  • Apparent Density/Tap Density: High density (>50% of theoretical) indicates good packing efficiency, leading to higher final part density.
  • Low Moisture and Oxide Content: Powder must be stored and handled in a dry, controlled atmosphere (often in an argon environment) to prevent oxidation and hydrogen pickup, which can cause porosity in the printed parts.
5. Microstructure and Heat Treatment
As-Printed (As-Built) Condition:

The rapid cooling rates (~10^5 - 10^6 K/s) in LPBF create a very fine, non-equilibrium microstructure. It consists of a supersaturated aluminum matrix (α-Al) with an extremely fine cellular/dendritic network of silicon. This fine structure contributes to the good "as-printed" strength.

Heat Treatment (Post-Processing):

Heat treatment is used to tailor the mechanical properties for specific applications.

  • Stress Relief (T1): A low-temperature anneal (~300°C for 2 hours) to reduce internal residual stresses from the build process without significantly altering the microstructure.
  • Direct Aging (T5): The part is artificially aged (e.g., 160-180°C for 4-12 hours) directly after printing. This precipitates fine Mg₂Si particles within the matrix, increasing strength and hardness while minimizing distortion.
  • Solution Heat Treatment and Aging (T6): This is the most common treatment for maximum strength. The part is solutionized at a high temperature (~520-540°C), quenched, and then aged. This process coarsens the silicon network (reducing ductility slightly) but maximizes precipitation hardening, yielding the highest tensile strength and hardness.
6. Applications

AlSi10Mg is versatile and used across numerous industries:

  • Aerospace: Bracket components, satellite parts, drone frames, and non-structural cabin components.
  • Automotive: Lightweight brackets, engine components (e.g., intake manifolds), heat exchangers, and custom hydraulic fittings.
  • Industrial: Robotic end-effectors, jigs, fixtures, and lightweight automation components.
  • Thermal Management: Heat sinks, cold plates for electronics, and cooling channels for molds (conformal cooling).
  • Prototyping: Functional prototypes that require metal-like properties for testing.
7. Advantages and Limitations
Advantages:
  • Excellent printability and high build success rates.
  • Good specific strength (strength-to-weight ratio).
  • Favorable thermal properties.
  • Widely available and well-documented.
  • Cost-effective compared to other high-performance AM alloys (e.g., Scalmalloy®).
Limitations:
  • Moderate Ductility: Especially in the T6 condition, elongation at break is lower than some wrought aluminum alloys.
  • Not for High-Temperature Applications: Mechanical properties degrade significantly above ~200°C due to the coarsening of strengthening precipitates.
  • Anisotropic Properties: Mechanical properties can be slightly different in the vertical (build) direction compared to the horizontal direction due to the layer-by-layer nature of AM.
High Strength Weight Ratio AlSi10Mg Aluminum Alloy Powder For Additive Manufacturing  0 High Strength Weight Ratio AlSi10Mg Aluminum Alloy Powder For Additive Manufacturing  1

Send your inquiry directly to us

Privacy Policy China Good Quality Planetary Ball Mill Machine Supplier. Copyright © 2025 Guangzhou Zoli Technology Co.,Ltd. . All Rights Reserved.