Materials: Stainless Steel Alloy Metal Powder
Particle Size: 1-100 Microns
Features: High Wear Resistance, High Impact Toughness, Low Breakage Rate
Composition: Cr: 17-19%, Ni: 8-10%, C: 0.08%, Mn: 2%, Si: 1%, P: 0.045%, S: 0.03%
Powder Storage Conditions: Dry And Cool Environment
Available Metal Types: Stainless Steel, Aluminum, Titanium, Inconel, Cobalt Chrome, Etc.
Application: Grinding And Mixing
Type: Laboratory Equipment
Wear Resistance: High
Hardness: HRC 58-62
Size: 1mm, 2mm, 3mm, 4mm, 5mm, 6mm, 7mm, 8mm, 9mm, 10mm, 11mm, 12mm, 13mm, 14mm, 15mm
Density: 7.95 G/cm3
Chemical Composition: WC-Co
Wear Resistance: Superior
Surface Finish: Polished
Usage: For Laboratory And Industrial Use
Grinding Ball Diameter: 3mm, 5mm, 10mm, 15mm, 20mm
Safety Features: Overload Protection, Interlock Protection, Emergency Stop
Particle Size: 1-3 Microns
Country Of Origin: China
Corrosion Resistance: Ideal For Wet Grinding
Hardness (HRC): 20–25 (annealed) / 50–58 (hardened)
Chemical Composition: C: 0.08%, Si: 1.00%, Mn: 2.00%, P: 0.045%, S: 0.030%, Cr: 17.00-19.00%, Ni: 8.00-10.00%, N: 0.10%
Size: 1mm-50mm
Fe-Ni-Cr (17-4PH, 316L): 3D Printing
Density (g/cm³): 7.4–7.9 (varies By Alloy)
Melting Point: 1538 °C
Purity: 99%
Features: High Wear Resistance, Corrosion Resistance, And Impact Toughness
Density: 7.85g/cm3
Surface: Polished
Wear Rate: < 0.1%
Send your inquiry directly to us