logo
Rumah > Produk > Aluminium Metal Powder >
AlSi10Mg Aluminium Alloys In Additive Manufacturing And Laser Powder Bed Fusion Processes

AlSi10Mg Aluminium Alloys In Additive Manufacturing And Laser Powder Bed Fusion Processes

Tempat asal:

CINA

Nama merek:

Zoli

Sertifikasi:

ISO CE

Nomor model:

ALSI10MG

Hubungi Kami
Minta Kutipan
Rincian produk
Nomor CAS:
7429-90-5
Permukaan akhir:
Mulus
Aplikasi:
Aditif untuk paduan logam, bahan bakar roket, kembang api, reaksi termite, dll.
suhu sintering:
Tergantung pada paduan logam spesifik yang digunakan
Fitur:
Bubuk putih ramping
Kemurnian:
99,7%
Suasana Sintering:
Nitrogen atau hidrogen
Warna:
Perak
Titik lebur:
660.3°C
Standar:
GB/T 2085-2007
Luas permukaan spesifik:
1-3 m2/g
Bahan:
Aluminium
Kelas bahaya:
Tidak berbahaya
Aplikasi bedak:
Pencetakan 3D
pabrikan:
Guangzhou Zoli
Syarat Pembayaran & Pengiriman
Kuantitas min Order
1kg
Kemasan rincian
vakum, plastik, dan tong besi
Waktu pengiriman
dalam 30 hari
Syarat-syarat pembayaran
L/C, T/T, Western Union
Menyediakan kemampuan
500 ton per tahun
Deskripsi Produk
Detailed Description: AlSi10Mg Powder for Metal 3D Printing

AlSi10Mg is one of the most widely used and well-understood aluminium alloys in additive manufacturing (AM), particularly in Laser Powder Bed Fusion (L-PBF) processes.

1. Chemical Composition

The name "AlSi10Mg" directly describes its primary alloying elements:

  • Al (Aluminium): Base metal (approximately 90%).
  • Si (Silicon): ~9-11%. Silicon lowers the melting point, reduces shrinkage during solidification, improves fluidity, and enhances castability and weldability. It also contributes to strength.
  • Mg (Magnesium): ~0.2-0.45%. Magnesium enables precipitation hardening through the formation of Mg₂Si phases during heat treatment, significantly increasing the material's strength.

A typical composition table looks like this:

ElementWeight %Function
Al (Aluminium)BalanceBase metal, provides low density and good corrosion resistance.
Si (Silicon)9.0 - 11.0 %Improves fluidity, reduces melting point, enhances castability.
Mg (Magnesium)0.2 - 0.45 %Enables age hardening (strengthening).
Fe (Iron)≤ 0.55 %Impurity, but helps prevent sticking to die casts. Kept low to avoid brittle phases.
Mn (Manganese)≤ 0.45 %Counteracts the negative effects of iron.
Cu (Copper)≤ 0.05 %Impurity, kept very low to avoid negative impact on corrosion resistance.
Zn (Zinc)≤ 0.10 %Impurity.
Ti (Titanium)≤ 0.15 %Grain refiner.
Others (each)≤ 0.05 %-
Others (total)≤ 0.15 %-

Critical Impurity: Oxygen Content
For AM powders, the oxygen content is a crucial specification not listed in standard composition tables. High-quality powder will have an oxygen content < 200 ppm (parts per million). Low oxygen is vital to prevent the formation of oxides, which can create defects, reduce mechanical properties, and cause issues during printing.

2. Manufacturing Process: Gas Atomization

AlSi10Mg powder for AM is almost exclusively produced via Gas Atomization:

  • Melting: The raw AlSi10Mg alloy is melted in a induction furnace under a controlled atmosphere.
  • Atomization: The molten metal is poured through a tundish (a funnel) where a high-pressure stream of inert gas (usually Nitrogen or Argon) breaks the liquid stream into fine droplets.
  • Solidification: These droplets cool and solidify into spherical particles as they fall in the atomization tower.
  • Sieving and Classification: The powder is then sieved to achieve a specific Particle Size Distribution (PSD), crucial for 3D printing.

Key Powder Characteristics:

  • Morphology: Perfectly spherical particles are ideal. This ensures excellent flowability, which is critical for spreading thin, uniform layers in the powder bed.
  • Particle Size Distribution (PSD): The most common PSD for L-PBF is 15-45 μm or 20-63 μm. A tight distribution ensures consistent packing density and smooth recoating.
  • Satellites: Small particles that are welded to larger ones. High-quality powder has minimal satellites, as they can hinder flowability.
3. Material Properties (After Printing - L-PBF Process)

The L-PBF process creates a unique, fine microstructure that differs from traditionally cast AlSi10Mg.

As-Built (Directly after printing):

  • High Strength & Hardness: The rapid cooling (quenching) creates a super-saturated solution and a very fine cellular microstructure surrounded by a silicon network. This results in higher tensile strength and hardness compared to casting.
  • Relatively Low Ductility: The as-built material can be brittle.

After Heat Treatment (T6 - Solution Heat Treated and Aged):

  • Improved Ductility: Strength decreases slightly, but elongation at break increases significantly, making the part tougher and less brittle.
  • Stress Relief: Removes residual stresses from the rapid heating and cooling of the printing process.

Typical Mechanical Properties (L-PBF, Vertical Orientation):

PropertyAs-BuiltAfter T6 Heat TreatmentCast Equivalent (A360)
Tensile Strength350 - 450 MPa250 - 350 MPa~315 MPa
Yield Strength (0.2%)200 - 250 MPa150 - 230 MPa~165 MPa
Elongation at Break3 - 8 %6 - 12 %~4%
Hardness (HBW)115 - 135100 - 120~75

Other Properties:

  • Density: ~2.67 g/cm³ (The printed part is typically >99.5% dense)
  • Thermal Conductivity: ~120 - 150 W/m·K (good for heat exchangers)
  • Melting Point: ~570°C - 600°C (approx.)
4. Applications

AlSi10Mg is the go-to material for lightweight, functional components across industries:

  • Aerospace: Brackets, mounts, ducting, cabin components, satellite parts.
  • Automotive: Lightweight brackets, engine components (e.g., turbocharger housings), heat exchangers, and custom parts for motorsports.
  • Industrial: Robotic arms, end-effectors, jigs, fixtures, and tooling.
  • Thermal Management: Heat sinks and complex, optimized heat exchangers that are impossible to make traditionally.

Kirim pertanyaan Anda langsung ke kami