polished tungsten sphere (5) Online Manufacturer
Impact Toughness: High
Advantages: High Hardness, High Density, Excellent Wear Resistance
Density: 14.6 G/cm3
Heat Resistance: High
Thermal Expansion Coefficient: 10.5 X 10-6/°C
Density: 6.0 G/cm3
Cobalt-Bound (WC-Co): Up To 500°C
Nickel-Bound (WC-Ni): Up To 600°C
Crushing Load: ≥1000 N
Solubility: Insoluble In Water